The standard JB Weld can be used up to 260°C so it would be okay for powder coating. (takes a long time to harden though)

 

The JB Weld Kwik isn't as good at 150°C, might just be okay.

 

JB Stik will fully cure in 20-30 minutes , okay upto 260°C

 

I wish I could find a local supplier, I used to buy it at the local car accessory shop but when I wanted some a couple of years ago I couldn't find any locally anywhere, they all stopped selling it.

 

You can get it on Ebay but that's not ideal if you're in a hurry.

Link to comment
Share on other sites

Please sign in to comment

You will be able to leave a comment after signing in



Sign In Now
×
×
  • Create New...

Important Information

We have placed cookies on your device to help make this website better. You can adjust your cookie settings, otherwise we'll assume you're okay to continue. You might also be interested in our Guidelines, Privacy Policy and Terms of Use.